Hayes Metals

Call us: +61 2 9627 7150
You can have confidence in Hayes Metals.

DCB1 Die Casting Bronze

BS1400:1985

Composition

(maximum % unless otherwise listed)

Cu 59.0 - 62.0
Zn Remainder
Pb 0.25
Al 0.25 - 0.5
T-I 0.75

T-I Total Impurities

Elements marked with * are specified impurities

Typical Physical Properties

 

Tensile Strength (MPa) 280-370
Elongation (% min) 23-50
0.2% Proof Stress (MPa) 90-120
Hardness (HB) 60-70